Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.410 GPa | 59.5 ksi | (stiffness), ASTM D882 |
DuPont™ Clysar® HP Polyolefin Shrink Packaging Film, 60 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, linear low-density polyolefin film. Cross-linking produces a film that is extremely rugged and durab.. |
|||
Modulus of Elasticity | 0.410 GPa | 59.5 ksi | (stiffness), ASTM D882 |
DuPont™ Clysar® HP Polyolefin Shrink Packaging Film, 75 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, linear low-density polyolefin film. Cross-linking produces a film that is extremely rugged and durab.. |
|||
Modulus of Elasticity | 0.410 GPa | 59.5 ksi | (stiffness), ASTM D882 |
DuPont™ Clysar® HP Polyolefin Shrink Packaging Film, 100 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, linear low-density polyolefin film. Cross-linking produces a film that is extremely rugged and durab.. |
|||
Modulus of Elasticity | 0.410 GPa | 59.5 ksi | (stiffness), ASTM D882 |
DuPont™ Clysar® HP Polyolefin Shrink Packaging Film, 150 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, linear low-density polyolefin film. Cross-linking produces a film that is extremely rugged and durab.. |
|||
Modulus of Elasticity | 0.410 GPa | 59.5 ksi | (stiffness), ASTM D882 |
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 60 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of .. |
|||
Modulus of Elasticity | 0.410 GPa | 59.5 ksi | (stiffness), ASTM D882 |
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 75 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of .. |
|||
Modulus of Elasticity | 0.410 GPa | 59.5 ksi | (stiffness), ASTM D882 |
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 100 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of .. |
|||
Modulus of Elasticity | 0.410 GPa | 59.5 ksi | (stiffness), ASTM D882 |
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 150 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of .. |