Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.392 - 2.25 GPa | 56.9 - 326 ksi | Average value: 0.556 GPa Grade Count:42 |
Overview of materials for Polytetrafluoroethylene (PTFE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v.. |