Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.213 GPa | 30.9 ksi | ASTM D-638 |
Bapolene® 1072 Polyethylene, Injection Grade A high flow general purpose injection molding resin with good gloss, toughness and stress crack resistance. This product meets FDA standards for food contact applications.Applications: Housewares, .. |