Polymer Property : Modulus of Elasticity = 0.109 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.000750 GPa
0.109 ksi
10% Modulus, Cured 7 min at 177°C and Post Cured 16 hr at 232°C
DuPont Performance Polymers GBL-900 Formulation  (discontinued **)
FormulationViton® GBL-900