Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.0900 GPa | 13.1 ksi | |
AorTech Biomaterials ECSil™ 60D Biomedical Carbonate Silicone Pellets Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an.. |
|||
Modulus of Elasticity | 0.0900 GPa | 13.1 ksi | |
AorTech Biomaterials ECSil™ 60D Biomedical Carbonate Silicone Pellets Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an.. |
|||
Modulus of Elasticity | 0.0900 - 0.200 GPa | 13.1 - 29.0 ksi | Average value: 0.127 GPa Grade Count:12 |
Overview of materials for Low Density Polyethylene (LDPE), Masterbatch Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Masterbatch Grade". Each property range of values reported is minimum a.. |