Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.000600 GPa | 0.0870 ksi | 10% Modulus, Cured 7 min at 177°C and Post Cured 2 hr at 232°C |
DuPont Performance Polymers VTR 8650 (GBL-S) Peroxide Cured Fluoroelastomer (FKM) Formulation FormulationVTR 8650 |
|||
Modulus of Elasticity | 0.000600 GPa | 0.0870 ksi | 10% Modulus, Cured 7 min at 177°C and Post Cured 16 hr at 232°C |
DuPont Performance Polymers VTR GLT Peroxide Cured Fluoroelastomer (FKM) Formulation FormulationViton® VTR-8500 |
|||
Modulus of Elasticity | 0.000600 - 9.20 GPa | 0.0870 - 1330 ksi | Average value: 0.234 GPa Grade Count:42 |
Overview of materials for Thermoset Fluoroelastomer This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr.. |
|||
Modulus of Elasticity | 0.000600 GPa | 0.0870 ksi | 10% Modulus, Cured 7 min at 177°C and Post Cured 2 hr at 232°C |
DuPont Performance Polymers VTR 8500 (GLT-S) 8500 Peroxide Cured Fluoroelastomer (FKM) Formulation
(discontin FormulationViton® GLT |