Mechanical Properties Metric English Comments
Modulus of Elasticity 0.0443 GPa
6.43 ksi
ISO R527
Arkema Group Orevac® 9307 Y Film EVA-MAH Terpolymer
EVA Terpolymers based Main Applications: Extrusion coating Skin packaging adhesive Thermo-adhesive filmsInformation provided by Arkema Group