Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.0150 GPa | 2.18 ksi | DIN EN 826 |
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |