Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.01455 GPa | 2.110 ksi | initial; ASTM D1708 |
DSM Biomedical BioSpan® SPU Segmented Polyether Polyurethane (SPU) The flex life exhibited by BioSpan® SPU enables good performance in many different types of medical devices. This elastomeric polymer has shown the ability to withstand millions of flex cycles.The .. |