Mechanical Properties Metric English Comments
Modulus of Elasticity 0.00350 GPa
0.508 ksi
ISO 178
Premix Thermoplastics PRESEAL® TPE 5010
PRESEAL TPE 5010 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It may also find interesting uses as conductors or in grounding applica..