Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 92000 MPa
1.33e+7 psi
ISO 899-1
DSM Akulon® K230-HXG6 Nylon 6-30% Glass Reinforced (European Grade) (Cond)  (discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..