Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 430 MPa | 62400 psi | ISO 899-1 |
Polymer Industries Polyslick UHMW Rod Polyslick UHMW Rod exhibits all of the durable qualities of our Polyslick UHMW Sheet making it perfect for the application where sheet stock is not suitable. The material is ideally suited for the m.. |
|||
Tensile Creep Modulus, 1 hour | 430 MPa | 62400 psi | ISO 899-1 |
Polymer Industries Polyslick UHMW Sheet Polyslick UHMW Sheet exhibits the properties of excellent impact strength, abrasion resistance, low coefficient of friction, as well as very good chemical resistance. This industrial grade material .. |
|||
Tensile Creep Modulus, 1 hour | 430 MPa | 62400 psi | ISO 899-1 |
Polymer Industries Polyslick UHMW Profile Polyslick UHMW Profiles exhibit all of the durable qualities of our Polyslick UHMW Sheet making them perfect for use where sheet stock is not suitable. Polymer Industries offers a large variety of p.. |
|||
Tensile Creep Modulus, 1 hour | 430 MPa | 62400 psi | |
LyondellBasell Lupolen® 5261 Z HDPE, Blow Molding Grade Relatively high viscosity blow molding grade for rigid, stackable and highly shock resistant containers for packaging all types of hazardous materials such as flammable, corrosive, poisonous and sur.. |