Tensile Creep Modulus, 1 hour 370 - 550 MPa
53700 - 79800 psi
Average value: 446 MPa Grade Count:7
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i..