Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 450 MPa
65300 psi
LyondellBasell Lupolen® 5621 D HDPE
Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.