Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 30.7907 - 111.849 MPa @Temperature 40.0 - 100 °C |
4465.82 - 16222.4 psi @Temperature 104 - 212 °F |
Average value: 66.3 MPa Grade Count:1 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Tensile Creep Modulus, 1 hour | 30.7907 - 111.849 MPa @Pressure 0.500 - 7.00 MPa |
4465.82 - 16222.4 psi @Pressure 72.5 - 1020 psi |
Average value: 66.3 MPa Grade Count:1 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |