Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 25.0 MPa @Strain 0.345 %, Temperature 23.0 °C |
3630 psi @Strain 0.345 %, Temperature 73.4 °F |
50%RH; 10h; Isochronous; ISO 899 |
DuPont Performance Polymers Zytel® 70G30HSLR NC010 Nylon 66
(Unverified Data**) Zytel® 70G30HSLR NC010 is a 30% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Creep Modulus, 1 hour | 25.0 MPa @Strain 0.322 %, Temperature 23.0 °C |
3630 psi @Strain 0.322 %, Temperature 73.4 °F |
50%RH; 1h; Isochronous; ISO 899 |
DuPont Performance Polymers Zytel® 70G30HSLR NC010 Nylon 66
(Unverified Data**) Zytel® 70G30HSLR NC010 is a 30% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |