Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Creep Modulus, 1 hour = 2400 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 1400 - 2400 MPa
203000 - 348000 psi
Average value: 2120 MPa Grade Count:9
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an..
Copyright © lookpolymers.com All Rights Reserved