Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 2300 MPa
334000 psi
Arkema Group Oroglas® MI-4T Acrylic, Heat Resistant  (discontinued **)
OROGLAS MI-4T is an acrylic grade that associates improved impact resistance with high heat resistance.Key features improved impact resistance: up to 4 times more impact resistant than standard acr..
Tensile Creep Modulus, 1 hour 2300 MPa
334000 psi
ISO 899-1
Lanxess Pocan® S 7926 000000 PBT
PBT, non-reinforced, injection molding, extrusion, flame retardant, impact modified
Tensile Creep Modulus, 1 hour 2300 MPa
334000 psi
BASF Luranyl® KR 2402 Polyphenylene Ether + Styrene-Butadiene Blend, Impact Grade
Base grade with a balanced combination of impact strength and stiffness for parts calling for good heat deformation resistance (e.g. warm-air vents, coil formers, sheet and wheel covers).Data was co..
Tensile Creep Modulus, 1 hour 2300 MPa
334000 psi
ISO 899-1
Lanxess Pocan® S 7020 000000 PBT
PBT, non-reinforced, injection molding, extrusion, flame retardant, impact modified