Polymer Property : Tensile Creep Modulus, 1 hour = 194000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 1340 MPa

@Temperature 23.0 °C
194000 psi

@Temperature 73.4 °F
50%RH; ISO 899
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66  (Unverified Data**)
Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers
Tensile Creep Modulus, 1 hour 1340 MPa

@Time 3600 sec
194000 psi

@Time 1.00 hour
50%RH; ISO 899-1
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66  (Unverified Data**)
Unreinforced UV Stabilized Polyamide 66 Zytel 105F BK010 is a lubricated fast cycling weather resistant PA 66 resin. Zytel 105F BK010 contains finely dispersed carbon black.Information provided by D..