Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 1500 - 2900 MPa
218000 - 421000 psi
Average value: 2590 MPa Grade Count:11
Overview of materials for Acetal Homopolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values ..
Tensile Creep Modulus, 1 hour 1500 MPa
218000 psi
ISO 899-1
Covestro Makroblend® S 7916 Polycarbonate + PBT, Impact Grade
ISO 7792-1-PBT/PC,MHPR,-020(PBT+PC)-blendsimpact modifiedInjection molding gradeexcellent chemical resistancehigh toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessing..
Tensile Creep Modulus, 1 hour 1500 MPa

@Time 3600 sec
218000 psi

@Time 1.00 hour
ISO 899-1
DuPont Performance Polymers Delrin® 520MP NC010 Acetal (POM)  (Unverified Data**)
20% Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 520MP is a medium viscosity acetal homopolymer containing 20% Teflon PTFE Micropowder. It is designe..