Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 15.0 MPa @Strain 0.244 %, Temperature 80.0 °C |
2180 psi @Strain 0.244 %, Temperature 176 °F |
50%RH; 1h; Isochronous; ISO 899 |
DuPont Performance Polymers Zytel® 70G30HSLR NC010 Nylon 66
(Unverified Data**) Zytel® 70G30HSLR NC010 is a 30% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Creep Modulus, 1 hour | 15.0 MPa @Strain 0.259 %, Temperature 80.0 °C |
2180 psi @Strain 0.259 %, Temperature 176 °F |
50%RH; 10h; Isochronous; ISO 899 |
DuPont Performance Polymers Zytel® 70G30HSLR NC010 Nylon 66
(Unverified Data**) Zytel® 70G30HSLR NC010 is a 30% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Creep Modulus, 1 hour | 15.0 MPa @Strain 0.205 %, Temperature 23.0 °C |
2180 psi @Strain 0.205 %, Temperature 73.4 °F |
50%RH; 10h; Isochronous; ISO 899 |
DuPont Performance Polymers Zytel® 70G30HSLR NC010 Nylon 66
(Unverified Data**) Zytel® 70G30HSLR NC010 is a 30% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Creep Modulus, 1 hour | 15.0 MPa @Strain 0.190 %, Temperature 23.0 °C |
2180 psi @Strain 0.190 %, Temperature 73.4 °F |
50%RH; 1h; Isochronous; ISO 899 |
DuPont Performance Polymers Zytel® 70G30HSLR NC010 Nylon 66
(Unverified Data**) Zytel® 70G30HSLR NC010 is a 30% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |