Polymer Property : Tensile Creep Modulus, 1 hour = 10.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 10.0 MPa

@Strain 0.172 %,
Temperature 100 °C
1450 psi

@Strain 0.172 %,
Temperature 212 °F
50%RH; 10h; Isochronous; ISO 899
DuPont Performance Polymers Zytel® 70G30HSLR NC010 Nylon 66  (Unverified Data**)
Zytel® 70G30HSLR NC010 is a 30% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Creep Modulus, 1 hour 10.0 MPa

@Strain 0.169 %,
Temperature 80.0 °C
1450 psi

@Strain 0.169 %,
Temperature 176 °F
50%RH; 10h; Isochronous; ISO 899
DuPont Performance Polymers Zytel® 70G30HSLR NC010 Nylon 66  (Unverified Data**)
Zytel® 70G30HSLR NC010 is a 30% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Creep Modulus, 1 hour 10.0 MPa

@Strain 0.159 %,
Temperature 80.0 °C
1450 psi

@Strain 0.159 %,
Temperature 176 °F
50%RH; 1h; Isochronous; ISO 899
DuPont Performance Polymers Zytel® 70G30HSLR NC010 Nylon 66  (Unverified Data**)
Zytel® 70G30HSLR NC010 is a 30% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Creep Modulus, 1 hour 10.0 MPa

@Strain 0.167 %,
Temperature 100 °C
1450 psi

@Strain 0.167 %,
Temperature 212 °F
50%RH; 1h; Isochronous; ISO 899
DuPont Performance Polymers Zytel® 70G30HSLR NC010 Nylon 66  (Unverified Data**)
Zytel® 70G30HSLR NC010 is a 30% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers