Tensile Creep Modulus, 1 hour 5000 - 7500 MPa
725000 - 1.09e+6 psi
Average value: 6430 MPa Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..