Polymer Property : Tensile Creep Modulus, 1 hour = 1.02e+6 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 7000 MPa
1.02e+6 psi
ISO 899-1
Lanxess Durethan® AKV 35 H2.0 901510 Nylon 66, 35% Glass Fiber
PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistanceApplication Examples: gearbox oil sumps, oil modules
Tensile Creep Modulus, 1 hour 7000 MPa
1.02e+6 psi
ISO 899-1
Lanxess Durethan® AKV 35 H2.0 SR1 901510 Nylon 66, Glass Fiber Reinforced
PA 66, 35% glass fibers, injection molding, heat-aging stabilized, improved surface finishInformation provided by LANXESS.
Tensile Creep Modulus, 1 hour 7000 MPa
1.02e+6 psi
ISO 899-1
Lanxess Durethan® AKV 35 H3.0 000000 Nylon 66, 35% Glass Fiber
PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistance