Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 209.3 kJ/m² | 99.59 ft-lb/in² | At 23°C; ASTM D1822S |
DuPont Nucrel® 2940 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2940is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |