Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 96.6 kJ/m² | 46.0 ft-lb/in² | ASTM D-1822 |
Axiall HHP-190 Rigid PVC, Extrusion Georgia Gulf HHP-190 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Heat Resistance & Thermal StabilityImpact Strength & ToughnessDimensi.. |