Mechanical Properties Metric English Comments
Tensile Impact Strength 640 kJ/m²
305 ft-lb/in²
Type S; ASTM D1822
SABIC Innovative Plastics Lexan® OQ2720 PC
Ophthalmic/safety lens market. OQ2xxx series in all transparent tints. Dedicated equipment, stringent production control conditions.
Tensile Impact Strength 640 kJ/m²
305 ft-lb/in²
Type S; ASTM D1822
SABIC Innovative Plastics Lexan® OQ2720 PC (Asia Pacific)
Ophthalmic/safety lens market. OQ2xxx series in all transparent tints. Dedicated equipment, stringent production control conditions.