Polymer Property : Tensile Impact Strength = 606 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 606 kJ/m²
288 ft-lb/in²
23°C; ASTM D-1822
ExxonMobil Escorene® LD-721 High EVA Coextrusion Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer specialty film resin providing outstanding heat sealability along with excellent strength, properties and clarity.App..
Tensile Impact Strength 606 kJ/m²
288 ft-lb/in²
At 23°C; ASTM D1822S
DuPont Nucrel® 960 Ethylene-Methacrylic Acid Copolymer Resin
Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for ..