Mechanical Properties Metric English Comments
Tensile Impact Strength 12.8 kJ/m²
6.10 ft-lb/in²
ASTM D-1822
Axiall 3802 Vinyl Foam, Extrusion
Georgia Gulf 3801, 3802, and 3803 are vinyl foam compounds designed for applications requiring lower density than standard rigid vinyls.Information provided by Georgia GulfGeorgia Gulf became Axiall..
Tensile Impact Strength 12.8 kJ/m²
6.10 ft-lb/in²
ASTM D-1822
Axiall 3801 Vinyl Foam, Extrusion
Georgia Gulf 3801, 3802, and 3803 are vinyl foam compounds designed for applications requiring lower density than standard rigid vinyls.Information provided by Georgia GulfGeorgia Gulf became Axiall..
Tensile Impact Strength 12.8 kJ/m²
6.10 ft-lb/in²
ASTM D-1822
Axiall 3803 Vinyl Foam, Extrusion
Georgia Gulf 3801, 3802, and 3803 are vinyl foam compounds designed for applications requiring lower density than standard rigid vinyls.Information provided by Georgia GulfGeorgia Gulf became Axiall..