Polymer Property : Tensile Impact Strength = 590 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 590 kJ/m²
281 ft-lb/in²
23°C; ASTM D-1822
ExxonMobil Optema® TC-221 Ethylene Methyl Acrylate for Compounding  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.27% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be used for making alloys, blends, and compounds, or be injection molded where..
Tensile Impact Strength 590 kJ/m²
281 ft-lb/in²
At 23°C; ASTM D1822
DuPont Elvax® 670 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Tensile Impact Strength 590 kJ/m²
281 ft-lb/in²
At -20°C; ASTM D1822
DuPont Elvax® 360 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..