Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 1190 kJ/m² | 566 ft-lb/in² | ASTM D1822S |
DuPont™ Surlyn® 9520 Ionomer Resin, Zinc Surlyn® 9520 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |