Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 101 - 113 kJ/m² | 48.1 - 53.8 ft-lb/in² | Average value: 108 kJ/m² Grade Count:3 |
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |