Tensile Impact Strength 1000 kJ/m²
476 ft-lb/in²
MD; EN ISO 8256
Propex Fabrics Curv™ C100A Polypropylene/Polypropylene Thermoformable Composite
Curv™ key features include weight savings, total recyclability, no glass content, thermoformable, high impact strength, inertness, and abrasion resistance.Data provided by BP Amoco; Curv was spun o..
Tensile Impact Strength 1000 kJ/m²
476 ft-lb/in²
CD; EN ISO 8256
Propex Fabrics Curv™ C100A Polypropylene/Polypropylene Thermoformable Composite
Curv™ key features include weight savings, total recyclability, no glass content, thermoformable, high impact strength, inertness, and abrasion resistance.Data provided by BP Amoco; Curv was spun o..