Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 95.0 kJ/m² | 45.2 ft-lb/in² | S bar; ASTM D 1822 |
Chevron Phillips Marlex® 9512H - 9513H High Performance Series HDPE Blow Molding Resin Resin Type: linear copolymerCharacteristics: excellent physical properties, medium molecular weight distribution, wide range of processing conditions, good flow for injection blow molding applicatio.. |