Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 357 kJ/m² | 170 ft-lb/in² | ASTM D1822 |
ExxonMobil HDPE BA53-055 High Density Polyethylene Resin Product Description: BA53-055 is a high molecular weight, high density polyethylene copolymer.Availability: Latin America, North America and South America Additive: Antistatic: NoApplications: Dru.. |
|||
Tensile Impact Strength | 357 kJ/m² | 170 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow UNIVAL™ DMDC-6143 NT 7 High Density Polyethylene Resin (HDPE) Excellent parison melt strength / low sag Good extrudability / process-ability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDC-6143 NT 7 is a polymer with broad molecular weight distri.. |