Mechanical Properties Metric English Comments
Tensile Impact Strength 130 - 353 kJ/m²
61.9 - 168 ft-lb/in²
Average value: 221 kJ/m² Grade Count:4
Overview of materials for Medium Density Polyethylene (MDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim..