Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 690 kJ/m² | 328 ft-lb/in² | 23°C; ASTM D-1822 |
ExxonMobil Escorene® LD-769 High EVA Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymer designed for high filler acceptance. Compounds produced from this resin have excellent flexibility and toughness.Appl.. |