Polymer Property : Tensile Impact Strength = 268 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 42.0 - 268 kJ/m²
20.0 - 128 ft-lb/in²
Average value: 155 kJ/m² Grade Count:6
Overview of materials for Polyphenylene Ether, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap..