Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 256 kJ/m² @Temperature -40.0 °C |
122 ft-lb/in² @Temperature -40.0 °F |
ASTM D1822 |
ExxonMobil LL 6100 Injection Molding Resin