Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 50.0 - 4800 kJ/m² | 23.8 - 2280 ft-lb/in² | Average value: 276 kJ/m² Grade Count:65 |
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum.. |