Mechanical Properties Metric English Comments
Tensile Impact Strength 451 kJ/m²
215 ft-lb/in²
ASTM D1822
Formosa Plastics Formolene® DB5305A Blow Molding HDPE  (discontinued **)
Extra High Molecular Weight Polyethylene Formolene® DB5305A is tailored for large part blow molding applications. Besides having excellent chemical resistance properties Formolene® DB5305A HDPE ha..