Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 205 kJ/m² | 97.5 ft-lb/in² | Notched, 23°C; ISO 8256 |
Total Finathene® 6006 HDPE, blow molding, pipe
(discontinued **) Finathene® 6006 is a high density polyethylene produced by the slurry loop low pressure polymerization process. Polymerization is conducted in the absence of any other comonomer. Finathene® 6006 h.. |