Polymer Property : Tensile Impact Strength = 178 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 178 kJ/m²
85.0 ft-lb/in²
ASTM D-1822
Axiall 9202J Rigid PVC, Molding
Georgia Gulf 9202J is suitable for all types of food packaging. The compound provides low taste and odor properties and contains an ultraviolet light stabilizer which protects light sensitive produ..