Polymer Property : Tensile Impact Strength = 148.5 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 311.8 kJ/m²

@Temperature -40.0 °C
148.5 ft-lb/in²

@Temperature -40.0 °F
ASTM D1822
ExxonMobil HD 6908.18 Injection Molding Resin  (discontinued **)
HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requiring very high stif..