Polymer Property : Tensile Impact Strength = 10.5 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 10.5 kJ/m²
5.00 ft-lb/in²
ASTM D1822
Ensinger DELRIN® AF DE588 Acetal Homopolymer, 20% PTFE filled (POM)
DELRIN® AF DE588 is a 20% PTFE filled homopolymer acetal that is fully tested and certified for use by the United States Navy. The resin is manufactured by DuPont and is used extensively in a varie..