Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.03136 GPa | 4.548 ksi | JIS K6301 |
Stellarchem GP-9401 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |