Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0313 GPa | 4.54 ksi | ASTM D412 |
Dow PELLETHANE® 2103-75D Film Grade Thermoplastic Polyurethane Elastomer
(discontinued **) Description: PELLETHANE® 2103-75D UV stabilized, polyether based thermoplastic polyurethane elastomer has excellent hydrolytic stability and excellent resistance to micro-organisms. Applications in.. |