Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0290 GPa | 4.21 ksi | ISO 37 |
AlphaGary Evoprene™ 081 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |