100% Modulus 0.0280 GPa
4.06 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1172 Polyester Based TPU
Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd.