Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0181 GPa | 2.63 ksi | ASTM D412-80 |
DuPont Performance Polymers Hypalon® 48 Chlorosulfonated Polyethylene Rubber, Peroxide Cured Carbon Black Filled Compound Carbon black compound with 100 parts Hypalon; 40 parts carbon black; 20 parts magnesia; and 5.8 parts Varox® DBPH-50. Physical property data below (except mooney viscosity) are for vulcanizate. Ma.. |